Guangxi Senhe High Technology Co.,Ltd.

Dedicated to Eco-friendly Gold Extraction

Russia GTY Gold Mine

Cases/More Cases

Phase

Monemer and bare gold

Gold in sulfide and asenide

Gold in gauge

Total

Content(%)

1.4

0.25

0.25

1.91

Occupancy(%)

73.3

13.61

13.09

100

After pre-treatment (with auxiliary agents),the wet process heap leaching was used and the recovery rate can reach 83.5%.